Determination of depth of decarburization

Accredia not accredited test:

Determination of depth of decarburization by the micro-hardness method according to UNI EN ISO 3887:2006 with determination of the total decarburizing depth.

 

Application field:

Hardened and tempered steel parts.

 

Sample requirements:

Optimal size: 20 x 20 x 20 mm